This is the main variable that determines the characteristics of HDPE, although the four mentioned variables do interact with each other. Ethylene is the main raw material of polyethylene, and a few other comonomers, such as 1-butene, 1-hexene or 1-octene, are also often used to improve polymer properties. For HDPE, the content of these few monomers is generally not more than 1%-2%. The addition of comonomer slightly reduces the crystallinity of the polymer. This change is generally measured by density, which is linearly related to crystallinity. The general classification in the United States is stipulated in ASTM D1248, and the density of HDPE is 0.940g/. C above; medium density polyethylene (MDPE) density range 0.926 ~ 0.940g/CC. Other classifications sometimes classify MDPE as HDPE or LLDPE. Homopolymers have the highest density, greatest stiffness, good permeation resistance, and highest melting point, but generally have poor environmental stress cracking resistance (ESCR). ESCR is the ability of PE to resist cracking caused by mechanical or chemical stress. Higher densities generally improve mechanical strength properties such as tensile strength, stiffness, and hardness; thermal properties such as softening point temperature and heat distortion temperature; and barrier properties such as air permeability or water vapor permeability. The lower density improves its impact strength and E-SCR. Polymer density is primarily affected by comonomer addition, but to a lesser extent also by molecular weight. A high molecular weight percentage reduces the density slightly. For example, homopolymers have different densities over a broad molecular weight range.